From: Selective synthesis of pure cobalt disulfide on reduced graphene oxide sheets and its high electrocatalytic activity for hydrogen evolution reaction
Concentration of GO (mg/mL)
Ratio of GO:Co2+ (mg:mmol)
Synthesized phase
0
0:1
CoS2Â +Â Co3S4Â +Â Co3O4Â +Â CoS
0.2
8.8:1
CoS2Â +Â Co3S4Â +Â CoS
1
44:1
CoS2Â +Â CoS
1.6
70.4:1
2
88:1
CoS2
2.3
101.2:1
2.6
114.4:1
4
176:1