Fig. 1

(*Reproduced with permission from Phaniraj et al. [12]. Copyright 2015 Elsevier)
SEM micrographs of the steels after hot rolling and interrupted cooling: a CMn, b 1.7 Cu, c TiMo*, d 1.7 CuTiMo
(*Reproduced with permission from Phaniraj et al. [12]. Copyright 2015 Elsevier)
SEM micrographs of the steels after hot rolling and interrupted cooling: a CMn, b 1.7 Cu, c TiMo*, d 1.7 CuTiMo