Fig. 3From: Formation of yttria-stabilized zirconia nanotubes by atomic layer deposition toward efficient solid electrolytesXRD patterns of YSZ-NT arrays from beam line 5 A with the wavelength 0.7653 Å using Mar 345-image plate at Pohang Light Source (South Korea). For converting image to the 2D diffraction pattern, FIT2D program was used. The 2θ of XRD pattern was recalculated to the corresponding angles of λ = 1.54 Å (Cu-Kα radiation)Back to article page