Skip to main content

Table 1 Heterogeneous reduction of substituted nitroaromatics catalyzed by CuO–GO nanocomposite catalyst in aqueous solution

From: Copper oxide–graphene oxide nanocomposite: efficient catalyst for hydrogenation of nitroaromatics in water

  1. Reaction conditions: nitroaromatics (1 mmol), NaBH4 (1.2 mmol), 30 min, CuO–GO nanocomposite catalyst (50 mg), aqueous solution. The yields were determined by GC–MS