From: Biomimetic anti-inflammatory and osteogenic nanoparticles self-assembled with mineral ions and tannic acid for tissue engineering

Fig. 6

a Alizarin red S staining images of hADSCs cultured with or without mTNs for 14 days (scale bar = 5 mm) and b quantitative analysis. c ALP activity of hADSCs cultured with GM and ODM with or without mTNs for 7 days. *Significantly different compared to GM (p < 0.05). Relative mRNA expression of the osteogenic markers (d) OPN, (e) RUNX2, and (f) OCN in hADSCs cultured in ODM with or without H2O2 and mTNs for 14 days. ∗, ∗ ∗, ∗ ∗ ∗significantly different compared to H2O2 (−)/mTN (−) (∗p < 0.033, ∗ ∗p < 0.002, ∗ ∗ ∗p < 0.001)